OCTG 9.625″ 53.5# 13CR80 Vam 21 SC80 SB R3

In transit to Coevorden. 13 Chrome L80, UNS S42000, is a quenched and tempered martensitic stainless steel used for corrosion resistance in sweet (CO2) and mildly sour (H2S) environments up to 300°F. Commonly used as downhole tubular components, packers, and other subsurface equipment, it is included in API 5CT as Group 2, Grade L80, Type 13Cr. Its controlled yield strength and hardness comply with NACE MR0175. This grade is best suited for mildly corrosive conditions as pH, chlorides, temperature, and H2S may limit its use. NACE MR0175/ISO15156 Table A.19 provides a recommended limit of 1.5 psi partial pressure H2S with pH ≥3.5.

Available Quantity

2,320

FT

Condition

Unused

Mill Year

Manufacturer

Location

Coevorden, Netherlands

Field Inspection

Completed!

Receiving Inspection

In Progress

Final Inspection

Not Started

Certified Report

Not Started

Field Inspection Complete!

In this first step of our PipeFacts™ quality assurance process, we send our field services team to inspect material in its stocked location. During the initial evaluation, we ensure that this material is suitable for acquisition and suitable for prime applications. Once the field inspection is complete, we move material to one of our regional storage and inspection hubs for further inspections.

What is

Field Inspection

?

10%
  • Traceability to MTR's
5%
  • Visual Body Inspection (VBI)
  • Visual thread Inspection (VTI)
  • Tally
  • Drift

Size

Nominal OD

9.625

in.

Nominal ID

8.535

in

Nominal Wall Thickness

0.545

in

Drift

8.379

in

Special Drift

8.5

in

Strength

Minimum Yield Strength

80

KSI

Minimum Ultimate Tensile Strength

95

KSI


Collapse Pressure

6,620

PSI

Internal / Burst Pressure

7,930

PSI

Disclaimer: The burst and collapse figures displayed are based on the API dimension tolerance of 87.5% of nominal wall thickness. Note that martensitic, duplex, super duplex, and nickel alloys often have tighter dimensional tolerances, therefore, increased strength ratings. The properties do not factor connection performance ratings. If your application requires more information ratings, please contact our technical services team, and we happily assist you.

Alloy

13CR

Family

Martensitic Stainless

Corrosion Resistance Level

Mild

Alloy Description

13 Chrome is a quenched and tempered martensitic stainless steel primarily used for corrosion resistance in environments with CO2 (sweet) and mild H2S (sour) exposure, with an operational temperature limit of up to 300°F. It is commonly applied in downhole tubular components, packers, and other subsurface equipment. This material is included in API 5CT as Group 2, Grade L80, Type 13Cr, and its yield strength and hardness are controlled to meet NACE MR0175 requirements.

While 13 Chrome L80 offers effective resistance in mildly corrosive conditions, its performance can be limited by factors such as pH, chloride concentration, temperature, and H2S content. According to NACE MR0175/ISO 15156, it is recommended for environments with a maximum H2S partial pressure of 1.5 psi and a pH ≥ 3.5 (refer to Table A.19).

Elemental Composition

C
6
Carbon
0.15%‒0.22%
Si
14
Silicon
1%
P
15
Phosphorus
0.02%
S
16
Sulfur
0.01%
Cr
24
Chromium
12%‒14%
Mn
25
Manganese
0.25%‒1%
Fe
26
Iron
83%‒87.6%
Ni
28
Nickel
0.5%
Cu
29
Copper
0.25%

Name

VAM 21 SC 80

Licensee

VAM

Category

Premium

Thread Type

Threaded & Coupled

Description